Chalking - Cameleon Paints | Industrial Coatings | Protective Coatings | Toll Manufacturing | Textured Coatings

Cameleon Paints
Specialists in Coatings & Paint Manufacturing!
Phone: 08 9302 2577 Email Enquiry

CHALKING

 

 

 

 

 

"Formation of fine powder on the surface of the paint film during weathering which can cause colour fading. Although some degree of chalking is a normal, desirable way for a paint film to wear, excessive film erosion can result from heavy chalking."

 

 

 

 

 

 

POSSIBLE CAUSES:

 

1. Use of a low-grade, highly pigmented paint.

2. Use of an interior paint for an outdoor application.

 

 

SOLUTION:

 

First, remove as much of the chalk residue as possible, scrubbing with a stiff bristle brush (or wire brush on masonry) and then rinse thoroughly; or use power washing equipment. Check for any remaining chalk by running a hand over the surface after it dries. If noticeable chalk is still present, apply a quality oil-based or acrylic latex primer (or comparable sealer for masonry), then repaint with a quality exterior coating; if little or no chalk remains and the old paint is sound, no priming is necessary

Products & Services Products & Services

Get the most from your Paints and Coatings, find out how with this FREE Report
Download
Contact Us:
26 Paramount Drive
Wangara WA  6065
Ph: 08 9302 2577
Fax: 08 9302 2578
Email Enquiry Map Details
 
Copyright © 2012 Cameleon Paints All Rights Reserved | Partners | GTP Web Design Perth